Inconel Wire

Check up to five results to perform an action.

Copper Wire

larger image





    border="0" Printable Page  
    Email Email This Page  
    Save To Favorites Save To Favorites
  
Request InformationCompare Items   Results Per Page : 
  Results 1 - 5 of 5 1 

Item #

Approx. Chemical Composition

Density

Melting Point

Coefficient of Expansion

Standards

Approx. Tensile Strength

Rigidity Modulus

Young's Modulus

Approx. Service Temperature

Manufacturer

Heat Treatments

Inconel 600 Wire Ni (>72%), Cr (14-17%), Fe (6-10%) 8.47 g/cm³ 1413 °C 13.3 μ m/m °C At 21-93°C AMS 5687
ASTM B166
BS 3075 & 6 NA14
600-700 N/mm² (Annealed)
900-1150 N/mm² (Spring Temper)
75.6 kN/mm² 206 kN/mm² -200 to +340 °C PSW N/A
Inconel 601 Wire Ni (58-63%), Cr (21-25%), Fe (BAL), Al (1.0-1.7%) 8.11 g/cm³ 1411 °C 13.75 μ m/m °C at 20 - 100°C ASTM B166 1200-1450 N/mm² (Spring Temper)
700-900 N/mm² (Annealed)
81.2 kN/mm² 206.5 kN/mm² -200 to +340°C (for lightly stressed applications) PSW Stress relieve 480-870 °C (900-1600°F) for 1 hour and air cool (temperature depends on composition and amount of cold work)
Inconel 625 Wire Ni (>58%), Cr (20-23%), Mo (8-10%), Nb (3.15-4.15%), Fe (5%) 8.44 g/cm³ 1350 °C 12.8 μ m/m °C At 21-93°C BS 3076 NA21 1300-1600 N/mm² (Spring Temper)
800-1000 N/mm² (Annealed)
79.0 kN/mm² 205.8 kN/mm² -200 to +340°C
Spring Temper + stress relieved, springs can operate up to 200°C
PSW Spring Temper - Stress relieve at 260-370°C - 30-60 mins
Inconel 718 Wire Ni (50-55%), Cr (17-21%), Fe (BAL), Nb (4.75-5.5%), Mo (2.8-3.3%), Ti (0.65-1.15%), Al (0.2-0.8%) 8.19 g/cm³ 1336 °C 13.0 μ m/m °C At 21 - 93°C AMS 5962
ASTM B637
1000 - 1200 N/mm² (No. 1 Temper)
1400 - 1600 N/mm² (Aged)
77.2 kN/mm² 204.9 kN/mm² No. 1 Temper aged -200 to +550 °C PSW
No. 1 Temper Solution anneal at 980 °C-1 Hrs-A/C
+
Age at 720 °C - 8 Hrs - F/C to 620 °C
hold at 620 °C so total age time is 18 Hrs air cool
Inconel X750 Wire Ni (>70%), Ti (2.25-2.75%), Cr (14-17%), Al (0.4-1.0%), Fe (5-9%), Nb (0.7-1.2%) 8.28 g/cm³ 1430 °C 12.6 μ m/m °C at 21-93°C AMS 5698 (No. 1 Temper)
AMS 5699 (Spring Temper)
ASTM B637
BS HR505
3 part Heat Treated - 1100-1250 N/mm²
Aged - 1300-1450 N/mm2
Aged - 1350-1750 N/mm2
No. 1 Temper - 900-1150 N/mm2
Spring Temper - 1100-1500 N/mm2
75.8 kN/mm² 213.7 kN/mm² No. 1 Temper aged - up to 550°C
Spring Temper + 3 Pt HT - up to 550°C
Spring Temper + age - up to 370°C
PSW No. 1 Temper - Age at 732°C - 16 Hrs - A/C|Spring Temper - Age at 650°C - 4 Hrs - A/C|Spring Temper - Solution anneal at 1150°C - 2 Hrs - A/C|(3 Pt HT) - + Stabilize at 843°C-24 Hrs-A/C|+ Precipitation harden at 704°C-20 Hrs-A/C